EN 10219-s355j2h steel pipe
TUSPIPE’s EN 10219 standard steel pipes are certified and meet the requirements of the EN 10219 standard in terms of material, dimensional tolerances, chemical composition, and mechanical properties.
EN 10219
그리고 European Norm EN 10219 regulates requirements for cold-formed welded structural pipes made of non-alloy and fine-grain steels without heat treatment. These requirements include dimensions, shapes, delivery conditions, and permissible deviations from dimensional and form tolerances, as well as mechanical property requirements. The standard applies to welded pipes used for the construction of steel structures and for the general purpose of civil engineering, including pipework for the transportation of fluid and other media. This standard also applies to welded pipes used in the construction of pipelines for the transportation of fluids such as oil, gas, and water. The standard is also applicable to welded pipes used in the construction of process piping, power piping, and ductwork. Part 1 includes the technical delivery conditions of EN 10219 structural pipes, and part 2 specifies the tolerance, dimensions and sectional properties of these pipes.
Steel Grade of EN 10219
Below is the steel grade of EN 10219 – S235JRH/ S275J2H/ S355J2H/ S275J0H/ S355J0H/ S355K2H. for TUSPIPE, quality is greater than everything. About the naming rules of steel grade, there are also examples to explain, so that you can better choose the products you need, if you have any questions you can contact us!

S235JRH
수율 강도: min. 235 MPa Application: Commonly used for structural and mechanical components with good weldability and formability. Impact Toughness: There is no specific impact toughness requirement for this grade.

S275J0H
수율 강도: Minimum 275 MPa Scope of application: Compared to S235JRH, it has higher strength and is suitable for structures subjected to higher loads. Impact Toughness: J0 indicates guaranteed impact performance at 0°C.

S275J2H
수율 강도: Minimum 275 MPa
Range of application: Same strength as S275J0H, but more suitable for low temperatures.
Impact Toughness: J2 indicates guaranteed impact performance at -20°C.

S355J0H
수율 강도: 355 MPa minimum Application: High-strength steel for structures carrying heavy loads, such as large buildings and projects. Impact toughness: J0 indicates guaranteed impact properties at 0°C.

S355J2H
수율 강도: Minimum 355 MPa
Range of application: Same strength as S355J0H, but for lower temperature environments.
Impact Toughness: J2 indicates guaranteed impact performance at -20°C.

S355K2H
Yield Strength: Minimum 355 MPa Application: Same strength as S355J0H and S355J2H, but provides higher impact toughness and better minimum impact energy. Impact Toughness: K2 indicates a higher guaranteed impact performance at -20°C.
Designation for EN 10219 Non-alloy Steel Structural Hollow Section
- 이 유럽 표준 (EN 10219 사양);
- 구조용 강철을 나타내는 대문자 S입니다;
- 두께 ≤16mm에 대한 최소 지정 항복 강도의 표시는 N/mm2로 표시됩니다;
- 상온에서 지정된 충격 속성을 가진 품질을 나타내는 대문자 JR입니다;
- 대문자 J와 숫자 0 또는 2는 각각 0℃ 및 -20℃에서 지정된 충격 특성을 가진 품질을 나타냅니다;
- 대문자 H는 속이 빈 섹션을 나타냅니다.
- Example with EN 10219 S275JOH:
- EN 10219 – Number of the 유럽 표준
- S – Structural steel
- 275 – Minimum yield strength (N/mm2) for thickness not greater than 16mm
- J0 – Impact properties, 27J minimum at 0℃
- H – Hollow section
Below you will find EN 10219 dimensions/mechanical properties/chemical composition/wall thicknesses and experimental data for tubing. This includes all EN 10219 standard steel grades that our manufacturers are able to produce. We hope you find them useful!
Weldability of EN 10219 Pipe
Weldable steels are specified in this European standard. EN 1011-1 and EN 1011-2 specify the main standards for welding products under this European standard.
When welding these products, the greatest danger is the development of cold cracking in the welded zone as the product thickness, strength level, and CEV rise. Cold cracking is a result of a combination of the following factors:
- elevated diffusible hydrogen levels in the weld metal;
- a brittle structure in the heat-affected zone;
- and large tensile stress concentrations in the welded joint
Dimensions and Sizes of EN 10219 Pipe
| DN | O. D. | W. T. | |||||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 인치 | mm | SCH5S | SCH10S | SCH10 | SCH20 | SCH30 | SCH40 | SCH60 | SCH80 | SCH100 | SCH120 | SCH140 | SCH160 | Sth | XS | XXS | |
| 50 | 2″ | 60.3 | 1.65 | 2.77 | - | - | - | 3.91 | - | 5.54 | - | - | - | 8.74 | 3.91 | 5.54 | 11.07 |
| 65 | 2 1/2″ | 73 | 2.11 | 3.05 | - | - | - | 5.16 | - | 7.01 | - | - | - | 9.53 | 5.16 | 7.01 | 14.02 |
| 80 | 3″ | 88.9 | 2.11 | 3.05 | - | - | - | 5.49 | - | 7.62 | - | - | - | 11.13 | 5.49 | 7.52 | 15.24 |
| 90 | 3 1/2″ | 101.6 | 2.11 | 3.05 | - | - | - | 5.74 | - | 8.08 | - | - | - | - | 5.74 | 8.08 | - |
| 100 | 4″ | 114.3 | 2.11 | 3.05 | - | - | - | 6.02 | - | 8.58 | - | 11.13 | - | 13.49 | 6.02 | 8.56 | 17.12 |
| 125 | 5″ | 141.3 | 2.77 | 3.4 | - | - | - | 6.55 | - | 9.53 | - | 12.7 | - | 15.88 | 6.55 | 9.53 | 18.05 |
| 150 | 6″ | 168.3 | 2.77 | 3.4 | - | - | - | 7.11 | - | 10.97 | - | 14.27 | - | 18.26 | 7.11 | 10.97 | 21.95 |
| 200 | 8″ | 219.1 | 2.77 | 3.76 | - | 6.35 | 7.04 | 8.18 | 10.31 | 12.7 | 15.09 | 18.26 | 20.62 | 23.01 | 8.18 | 12.7 | 22.23 |
| 250 | 10″ | 273.1 | 3.4 | 4.19 | - | 6.35 | 7.8 | 9.27 | 12.7 | 15.09 | 18.26 | 21.44 | 25.4 | 28.58 | 9.27 | 12.7 | 25.4 |
| 300 | 12″ | 323.9 | 3.96 | 4.57 | - | 6.35 | 8.38 | 10.31 | 14.27 | 17.48 | 21.44 | 25.4 | 28.58 | 33.32 | 9.53 | 12.7 | 25.4 |
| 350 | 14″ | 355.5 | 3.96 | 4.78 | 6.35 | 7.92 | 9.53 | 11.13 | 15.09 | 19.05 | 23.83 | 27.79 | 31.75 | 35.71 | 9.53 | 12.7 | - |
| 400 | 16″ | 406.4 | 4.19 | 4.78 | 6.35 | 7.92 | 9.53 | 12.7 | 16.66 | 21.44 | 26.19 | 30.96 | 36.53 | 40.49 | 9.53 | 12.7 | - |
| 450 | 18″ | 457.2 | 4.19 | 4.78 | 6.35 | 7.92 | 11.13 | 14.27 | 19.05 | 23.83 | 39.36 | 34.93 | 39.67 | 45.24 | - | - | - |
| 500 | 20″ | 508 | 4.78 | 5.54 | 6.35 | 9.53 | 12.7 | 15.09 | 20.62 | 26.19 | 32.54 | 38.1 | 44.45 | 50.01 | - | - | - |
| 550 | 22″ | 558.8 | 4.78 | 5.54 | 6.35 | 9.53 | 12.7 | - | 22.23 | 28.58 | 34.93 | 41.28 | 47.63 | 53.98 | - | - | - |
| 600 | 24″ | 609.6 | 5.54 | 6.35 | 6.35 | 9.53 | 14.27 | 17.48 | 24.61 | 30.96 | 38.89 | 46.02 | 52.37 | 59.54 | - | - | - |
Chemical Composition Requirement of EN 10219 Pipe
Please check the table below for the chemical composition requirement of EN 10219 structural hollow sections, thickness ≤ 40mm.
EN 10219 S235JRH/ S275J2H/ S355J2H/ S275J0H/ S355J0H/ S355K2H.
| 강철 등급 | Ytpe of De-oxidation a | % by Mass, Maximum | ||||||
|---|---|---|---|---|---|---|---|---|
| 강철 이름 | 스틸 번호 | C | Si | Mn | P | S | N b | |
| S235JRH | 1.0039 | FF | 0.17 | - | 1.40 | 0.040 | 0.040 | 0.009 |
| S275J0H | 1.0149 | FF | 0.20 | - | 1.50 | 0.035 | 0.035 | 0.009 |
| S275J2H | 1.0138 | FF | 0.20 | - | 1.50 | 0.030 | 0.030 | - |
| S355J0H | 1.0547 | FF | 0.22 | 0.55 | 1.60 | 0.035 | 0.035 | 0.009 |
| S355J2H | 1.0576 | FF | 0.22 | 0.55 | 1.60 | 0.030 | 0.030 | - |
| S355K2H | 1.0512 | FF | 0.22 | 0.55 | 1.60 | 0.030 | 0.030 | - |
| a The deoxidation method is designated as follws: FF: Fully killed steel containing nitrogen binding elements in amounts sufficient to bind available nitorgen (e.g. min. 0.020% total Al or 0.015% shluble Al). | ||||||||
| b The maximum value for nitrogen dose not apply if the chemical composition shows a minimum total Al content of 0.020% with a minimum Al/N ratio of 2:1, or if sufficient other -binding elements are present. The N-binding elements shall be reocrded in the Inspection Document. | ||||||||
Mechanical Properties of EN 10219 Pipe
The table below lists the required mechanical properties for EN 10219 structural hollow sections.
| 강철 등급 | Minimum Yield Strength ReH MPa | 인장 강도 Rm MPa | Minimum elongation Ad % | Minimum Impact Energy KVe J | |||||
|---|---|---|---|---|---|---|---|---|---|
| Steel 이름 | Steel Number | Specified Thickness mm | Specified Thickness mm | Specified Thickness mm | at Test Temperature of | ||||
| ≤16 | > 16 ≤ 40 | <3 | ≥3 ≤40 | ≤40 | -20℃ | 0℃ | 20℃ | ||
| S235JRH a | 1.0039 | 235 | 225 | 360-510 | 360-510 | 24 b | - | - | 27 |
| S275J0H a | 1.0149 | 275 | 265 | 430-580 | 410-560 | 20 c | - | 27 | - |
| S275J2H | 1.0138 | 27 | - | - | |||||
| S355J0H a | 1.0547 | 355 | 345 | 510-680 | 470-630 | 20 c | - | 27 | - |
| S355J2H | 1.0576 | - | - | - | |||||
| S355K2H | 1.0512 | 40 f | - | - | |||||
| a The impact properties are verified only when Option 1.3 is specified | |||||||||
| b For thicknesses > 3 mm and section sizes D/T < 15 (round) and (B+H)/2T < 12.5 (square and rectangular) the minimum elongation is by 2. For thicknesses > 3 mm the minimum value for elongation is 17 %. | |||||||||
| c For section size D/T < 15 (circular) and (B+H)/2T < 12.5 (square and rectangular) and minimum elongation is reduced by 2. | |||||||||
| d For thicknesses < 3 mm see 9.2.2. | |||||||||
| e For impact properties for reduced section test pieces see 6.7.2 | |||||||||
| f This value corresponds to 27J at -30℃ (see EN 1993-1-1). | |||||||||
Inspection of EN 10219 Hollow Sections of Non-alloy Steels
EN 10219 is tensile tested according to EN 10002-1 and Charpy impact tested according to EN 10045-1.
| 검사 요구 사항 | 검사 빈도 | |||
|---|---|---|---|---|
| 테스트 유형 | 비특이적 검사 | 특정 검사 | ||
| 필수 테스트 | 1 | 캐스트 분석 | 배송당 하나의 결과 항목 | 캐스트당 하나 |
| 2 | 인장 테스트 | 배송당 하나의 결과 항목 | 테스트 단위당 하나 (b) | |
| 3 | 다음 대상에 대한 충격 테스트 품질 J2 및 K2 전용 | 해당 없음 | 테스트 유닛당 1세트(B) | |
| 4 | 표면 상태 및 치수 | - | - | |
| 5 | 용접부 NDT | 해당 없음 | 모든 제품, 전체 길이 | |
| 선택 사항 테스트 | 6 | 제품 분석 | 해당 없음 | 테스트 단위당 하나 |
| 7 | 캐스트 분석 추가 요소 | 해당 없음 | 옵션 1.2 참조 | |
| 8 | 충격 테스트 품질 JR 및 J0 | 해당 없음 | 테스트 유닛당 1세트(B) | |
| b - 제조업체의 재량에 따라 세로 또는 가로 샘플. | ||||
INSPECTION OF EN 10219 HOLLOW SECTIONS OF Fine-grain Steels
| 검사 요구 사항 | 검사 빈도 | ||
|---|---|---|---|
| 테스트 유형 | 특정 검사 | ||
| 필수 테스트 | 1 | 캐스트 분석 | 캐스트당 하나 |
| 2 | 인장 테스트 | One per test unitF( b) | |
| 3 | 충격 테스트 | 테스트 유닛당 1세트(B) | |
| 4 | 표면 상태 및 치수 | - | |
| 선택 사항 테스트 | 5 | 용접부 NDT | 모든 제품, 전체 길이 |
| 6 | 제품 분석 | 테스트 단위당 하나 | |
| b - 제조업체의 재량에 따라 세로 또는 가로 샘플. | |||
Marking of EN 10219
Each of the square and rectangular hollow sections shall be marked with the following information.
- Specification designation
- Grade letter
- 차원
- Heat number
- Other customers requirement
왜 투스피프를 선택해야 하나요?
1998년부터 Tianjin United Steel Piping Co., Ltd(TUSPIPE)는 고품질의 라인 파이프를 공급하기 위해 노력해 왔습니다.
With over 500,000 tons annual production capacity, the company serves various fields and industries, such as oil & gas exploitation and transmission, ship & auto-building, water & electricity, environmental protection, mechanical engineering, infrastructure construction and etc.
TUSPIPE places a premium on product quality and rigorous product quality control. In order to maintain good product quality, the company has established a Test & Inspection Center since 2004. With a series of state-of-the-art tests and inspection equipment, the test & inspection center is able to perform the tensile tests, hydro tests, impact tests, DWTT, etc.